The plaster is detached while it has resistances

A. Not right or not at all preparations for the homogenization of the setting

B.Uneven absorbance of the setting

 

For more information contact us to provides you with the “MANUAL OF PLASTER APPLICATION”

See more solutions

Curved fissures
A. Bad preparation of the setting B.Discontinuity of…
Longitudinal fissures
A.Extended time of stirring the mixture in the…
Big and deep fissures increased with time
The masonry has “sat”.   For more information…